WELDING PROCEDURES
Here is a list of our basic welding procedures.
Follow us on:
| 1 | Bureau Veritas Procedures | ||
| WPS 6S-01 rev 0 | EH36 FCAW | ||
| WPS 6S-02 rev 0 | EH36 FCAW | ||
| WPS 6S-03 rev 0 | API 5L X52 GTAW/SMAW | ||
| WPS 6S-04 rev 0 | Stainless Steel GTAW | ||
| WPS 6S-05 rev 0 | Stainless Steel GMAW | ||
| WPS 6S-06 rev 0 | EH36 SMAW | ||
| WPS 6S-07 rev 0 | EH36 – Stainless Steel SMAW | ||
| WPS 6S-08 rev 0 | A106 Gr B GTAW | ||
| WPS 6S-09 rev 0 | Container Corner Cast Steel SMAW | ||
| WPQR C0585-1 | EH36 FCAW 25mm 2G | ||
| WPQR C0585-2 | EH36 FCAW 25mm 3G | ||
| WPQR C0585-3 | EH36 FCAW 8mm 2G | ||
| WPQR C0585-4 | EH36 FCAW 8mm 3G | ||
| WPQR C0585-5 | API 5L X52 GTAW/SMAW 8″NB 6G | ||
| WPQR C0585-6 | Stainless Steel GTAW 2″NB 6G | ||
| WPQR C0585-7 | Stainless Steel GMAW 6mm 2G | ||
| WPQR C0585-8 | EH36 SMAW 8mm 2G | ||
| WPQR C0585-9 | EH36 – Stainless Steel SMAW 8mm 2G | ||
| WPQR C0585-10 | A106 Gr B GTAW 2″NB 6G | ||
| WPQR C0585-11 | Container Corner Cast Steel SMAW 2G | ||
| WPQR C0585-12 | EH36 SMAW 8mm 3G | ||
| 2 | Lloyds Register of Shipping Procedures | ||
| WPS 6S-01 rev 0 | EH36 FCAW | ||
| WPS 6S-02 rev 0 | EH36 FCAW | ||
| WPS 6S-03 rev 0 | API 5L X52 GTAW/SMAW | ||
| WPS 6S-04 rev 0 | Stainless Steel GTAW | ||
| WPS 6S-05 rev 0 | Stainless Steel GMAW | ||
| WPS 6S-06 rev 0 | EH36 SMAW | ||
| WPS 6S-07 rev 0 | EH36 – Stainless Steel SMAW | ||
| WPS 6S-08 rev 0 | A106 Gr B GTAW | ||
| WPS 6S-09 rev 0 | Container Corner Cast Steel SMAW | ||
| WPQR C0585-1 | EH36 FCAW 25mm 2G | ||
| WPQR C0585-2 | EH36 FCAW 25mm 3G | ||
| WPQR C0585-3 | EH36 FCAW 8mm 2G | ||
| WPQR C0585-4 | EH36 FCAW 8mm 3G | ||
| WPQR C0585-5 | API 5L X52 GTAW/SMAW 8″NB 6G | ||
| WPQR C0585-6 | Stainless Steel GTAW 2″NB 6G | ||
| WPQR C0585-7 | Stainless Steel GMAW 6mm 2G | ||
| WPQR C0585-8 | EH36 SMAW 8mm 2G | ||
| WPQR C0585-9 | EH36 – Stainless Steel SMAW 8mm 2G | ||
| WPQR C0585-10 | A106 Gr B GTAW 2″NB 6G | ||
| WPQR C0585-11 | Container Corner Cast Steel SMAW 2G | ||
| WPQR C0585-12 | EH36 SMAW 8mm 3G | ||
| 3 | BV/LR NDE and MECHANICAL TEST Certificates | ||
| WPQR C0585-1 | RT, MPI, TT, BT, M/HT | ||
| WPQR C0585-2 | RT, MPI, TT, BT, MT, IT | ||
| WPQR C0585-3 | RT, MPI, TT, BT, M/HT | ||
| WPQR C0585-4 | RT, MPI, TT, BT, MT, IT | ||
| WPQR C0585-5 | RT, MPI, TT, BT, M/HT, IT | ||
| WPQR C0585-6 | RT, PT, TT, BT, MT | ||
| WPQR C0585-7 | RT, PT, TT, BT, MT | ||
| WPQR C0585-8 | RT, MPI, TT, BT, M/HT | ||
| WPQR C0585-9 | RT, PT, TT, BT, M/HT, IT | ||
| WPQR C0585-10 | RT, PT, TT, BT, MT, IT | ||
| WPQR C0585-11 | UT, MPI, M/HT | ||
| WPQR C0585-12 | RT, MPI, TT, BT, MT, IT | ||
| 4 | ASME IX Procedures | ||
| WPS 6S-01 rev 0 | EH36 FCAW | ||
| WPS 6S-02 rev 0 | EH36 FCAW | ||
| WPS 6S-03 rev 0 | API 5L X52 GTAW/SMAW | ||
| WPS 6S-04 rev 0 | Stainless Steel GTAW | ||
| WPS 6S-05 rev 0 | Stainless Steel GMAW | ||
| WPS 6S-06 rev 0 | EH36 SMAW | ||
| WPS 6S-07 rev 0 | EH36 – Stainless Steel SMAW | ||
| WPS 6S-08 rev 0 | A106 Gr B GTAW | ||
| WPS 6S-09 rev 0 | Container Corner Cast Steel SMAW | ||
| PQR C0585-2 | EH36 FCAW 25mm 3G | ||
| PQR C0585-4 | EH36 FCAW 8mm 3G | ||
| PQR C0585-5 | API 5L X52 GTAW/SMAW 8″NB 6G | ||
| PQR C0585-6 | Stainless Steel GTAW 2″NB 6G | ||
| PQR C0585-7 | Stainless Steel GMAW 6mm 2G | ||
| PQR C0585-9 | EH36 – Stainless Steel SMAW 8mm 2G | ||
| PQR C0585-10 | A106 Gr B GTAW 2″NB 6G | ||
| PQR C0585-11 | Container Corner Cast Steel SMAW 2G | ||
| PQR C0585-12 | EH36 SMAW 8mm 3G | ||
| 5 | ASME IX NDE and MECHANICAL TEST Certificates | ||
| PQR C0585-2 | RT, TT, BT, IT | ||
| PQR C0585-4 | RT, TT, BT, IT | ||
| PQR C0585-5 | RT, TT, BT, IT | ||
| PQR C0585-6 | RT, TT, BT | ||
| PQR C0585-7 | RT, TT, BT | ||
| PQR C0585-9 | RT, TT, BT, IT | ||
| PQR C0585-10 | RT, TT, BT, IT | ||
| TM C0585-13 | UT, MPI, M/HT | ||
| PQR C0585-12 | RT, TT, BT, IT | ||
| 6 | MATERIAL CERTIFICATES | ||
| EH36 25mm plate | |||
| EH36 8mm plate | |||
| API 5L Gr X52 8″NB x 12.7mm | |||
| ASME SA 312 Gr 316L 2″NB x 5.54mm | |||
| ASME SA 240 Gr 304L 6mm plate | |||
| ASME SA 240 Gr 304L 8mm plate | |||
| ASME SA 106 Gr B 2″NB x 5.54mm | |||
| SCW480 Cast Steel Corner Block | |||
| E71-T1 | 1.2mm FCAW wire | ||
| ER70S-6 | 2.4mm GTAW wire | ||
| E7018-1 | 2.5mm & 3.2mm SMAW electrodes | ||
| ER316L | 1.6mm GTAW wire | ||
| ER316L | 1.2mm GMAW wire | ||
| E309L | 3.2mm SMAW electrode |